The heat treatment of the anthracene fraction of coal tar under pressure is considered. In the production of synthetic pitch, the duration of the process is varied from 10 to 80 min, at a temperature of 500°C and a pressure of 3 MPa. Kinetic data for the formation of γ and α1 fractions show that the polycondensation of the γ fraction is of second order, while the formation of the α1 ...